Aluminium is easy to weld if you know its peculiarities: the tenacious oxide layer, the sensitivity to hydrogen, the high thermal conductivity and the tendency of some alloys to hot cracking. This series explains what matters in practice, based on standards, research reports and the experience of MIGAL.CO as a manufacturer of aluminium welding wire.
A good place to start is Welding aluminium: what is different from steel. The other articles follow the sequence of fabrication and can also be read individually.
Basics: what makes aluminium different
- Welding aluminium: what is different from steel: Heat conduction, distortion, oxide layer, porosity and wire feeding compared, with a selection table for the filler metal.
- Oxide layer: Why the thin oxide skin melts at around 2,050 °C and how to deal with it in welding.
- Solubility of hydrogen: Where porosity comes from: hydrogen that no longer stays dissolved during solidification.
- Condensation: When moisture condenses on cold workpieces and wire, and how to prevent it.
Preparation: surface, joint, temperature
- Surface preparation before welding: Storage, degreasing, removing oxide and whether the wire needs cleaning too.
- Joint preparation: Cutting, joint shapes by sheet thickness, a sound root, tacking and clamping.
- Preheating and interpass temperature: When preheating helps, when it costs strength, and which temperatures apply.
Welding: gas, wire, arc
- Gas shielded welding: Argon, helium and mixtures, gas flow, purge times and leak-tight lines.
- Wire feeding: How the soft aluminium wire gets from the drum or spool to the contact tip without problems.
- Arc ignition: Why aluminium ignites less easily than steel and what makes for reliable ignition.
- Weld start and end crater: Avoiding lack of fusion at the weld start and cracks in the end crater.
- Special points: Checklist for MIG and TIG equipment, castings and die castings, joints with steel.
Result: surface and weld quality
- Black deposit: Where the dark deposit beside the weld comes from and how to reduce it.
- Anodising: Why welds become discoloured when anodised and which filler matches in colour.
- Weld defects and how to avoid them: Porosity, oxide inclusions and hot cracks: causes and remedies at a glance.
Calculators and filler metals
- Material selector: which filler metal suits which base metal.
- Dew point calculator: when moisture condenses on the workpiece.
- Aluminium welding wire: all wires and rods with data sheets.
Frequently asked questions
What matters most when welding aluminium?
Cleanliness and dryness. Most defects, especially porosity and lack of fusion, are caused by oxide, moisture and dirt on the workpiece, wire and gas supply.
Which welding wire for aluminium?
That depends on the base metal and the requirements: strength, cracking sensitivity, colour after anodising. For 5000 series alloys usually AlMg fillers, for the 6000 series AlSi5 or AlMg5, for castings AlSi fillers. The material selector helps with the choice.
MIG or TIG for aluminium?
MIG is faster and is usually preferred in production, especially for thicker walls. TIG is suited to thin sheet, tubes and visible welds where weld appearance and precise heat control matter.
About the author
Robert Lahnsteiner, Ing., is an International Welding Engineer (IWE) and managing director of MIGAL.CO GmbH. After training in telecommunications and electronics at HTL Braunau, he spent eighteen years in welding technology at Fronius from 1983. Since 2001 he has run MIGAL.CO, the aluminium welding wire manufacturer in Landau an der Isar, together with Martin Erl. His focus is aluminium filler metals, wire manufacturing and wire feeding, and the monitoring of welding processes. Within DVS, the German Welding Society, he has served for around 30 years on technical committee FA03 “Arc welding” and chairs working group 2.4.4 “MIG welding of aluminium”.